TuoCore MagneticsCore & Magnetic Component Manufacturer

Materials & Grades

Choose by frequency, flux density and loss target. These are the grades we use most; other grades and gauges are available on request.

MaterialGradesThicknessTypical use
Silicon steel (GOES)23Q110 · 27Q100 · 30Q1200.23–0.30 mmLow core loss, high flux, 50/60 Hz
Silicon steel (NGOES)50W470 · 35W3000.35–0.50 mmLower cost, general purpose
Nanocrystalline1K107 (FeCuNbSiB)18–30 µmµi up to 100k+, lowest loss above 10 kHz
Amorphous2605SA1 (FeSiB)25 µmBs ≈ 1.56 T, low no-load loss
Ferrite MnZn (power)TC40 · TC44 · TC47 ≈ PC40 / PC44 / PC47—100 kHz – 1 MHz, power conversion
Ferrite MnZn (high-freq)TC90 · TC95 · TC96—High-frequency, low loss (server/EV power)
Ferrite NiZnHigh-frequency grade—1–500 MHz, EMI suppression

Frequency first

50/60 Hz → silicon steel. 10–100 kHz → nanocrystalline. 100 kHz–MHz → ferrite.

Flux and DC bias

Silicon steel Bs ≈ 2.0 T, amorphous 1.56 T, nanocrystalline 1.2 T, ferrite 0.4–0.5 T.

Loss vs cost

Thinner, higher-grade strip lowers loss but raises cost — balance against energy saved.